ES · EN · FR
 
Logotipo Tecnopol  
Productos y sistemas de impermeabilización y aislamiento
Tecnopol Sistemas
 

Timeouts

In the following tables, we facilitate the approximate waiting times between layers , since they can change according to the substrate and the weather.  If you have any  doubt contacts us and we will advise you at all times.

BEFORE APPLYING DESMOPOL ON DESMOPOL PRIMER-PU

Temperature of support
Minimum
Maximum
+10 ºC
3 hours
24-48 hours
+30 ºC
2 hours
+45 ºC
1 hour

 

BEFORE APPLYING DESMOPOL ON (REPAINTED) DESMOPOL

Temperature  of support
Minimum
Maximum
+10 ºC
24 hours
76 hours
+20 ºC
8 hours
+30 ºC 6 hours
+45 ºC
4 hours

 

BEFORE APPLYING DESMOPOL ADY ON DESMOPOL

Temperature of support
Minimum
Maximum
+10 ºC
6 hours
76 hours
+20 ºC
5 hours
+30 ºC 4 hours
+45 ºC
3 hours

 

CURED. PRODUCT READY FOR USE

Temperature of support
Resistance
to rain
Resistance
to pedestrian traffic
Resistance
to wheeled traffic
+10 ºC
60 minutes aprox.
48 hours
not resistant
without incorporation
of DESMOPOL ADY
+20 ºC
24 hours
+30 ºC
20 hours
+45 ºC
12 hours

 

 
     

certificaciones tecnopol

POLYUREA COATING SYSTEMS - POLYUREA COATING COMPANY 
Tecnopol, SL. - Pol. Ind. "Z" - C/ de la Prensa, 5 - CP: 08150 - Parets del Vallès (Barcelona)
Telf. 93 568 21 11 - Fax. 93 568 02 11 | E-mail: info@tecnopol.es | Legal Notice 
Tecnopol.es - Tecnocoat.es - Polyureacoatingsystems.com - Poliuretano.es

Manteniment informàtic Barcelona - Mantenimiento informático Valencia - Posicionamiento web